Versions Compared

Key

  • This line was added.
  • This line was removed.
  • Formatting was changed.

...

  1.  Speckling on the heater surface - Remained even after cleaning the surface with Alcohol - Maybe the flux spluttering and then baking on the heater surface
  2.  Over Soldering - We requested Tan to use lesser solder in the process. Could also be because there was a small gap between the wick and the heater surface causing the solder to flow. 

 

Test 3: May 14th  (Not successful)

...